[an error occurred while processing this directive]
基于同步辐射原位表征技术的镁合金研究进展
郭恩宇1,2(), 杜泽龙1, 李炳志1, 王同敏1,2()
Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques
GUO Enyu1,2(), DU Zelong1, LI Bingzhi1, WANG Tongmin1,2()

图4. 同步辐射X射线原位衍射技术在镁合金变形过程中的典型应用[53,55]

Fig.4. Typical applications of synchrotron radiation X-ray in situ diffraction technology in the deformation process of magnesium alloys
(a, b) {0002} pole figure of the extruded Mg97Y2Zn1 (atomic fraction, %) alloy (a) and evolution of intensity of various poles (b)[53] (ND—normal direction) (c, d) axial internal strains, overall sample strains, and intensity diffracted peaks during in situ compression at 100 oC (c) and 200 oC (d)[53] (e, f) orientation maps of the region of interest with 1 μm (e) and 2 μm (f) step sizes, respectively[55] (h'—height of mapping area)