基于同步辐射原位表征技术的镁合金研究进展
|
郭恩宇 1,2(  ), 杜泽龙 1, 李炳志 1, 王同敏 1,2(  )
|
|
Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques
|
GUO Enyu 1,2(  ), DU Zelong 1, LI Bingzhi 1, WANG Tongmin 1,2(  )
|
|
|
图3. 同步辐射原位四维成像技术揭示镁合金中的晶体生长与粗化机制[30,36]
|
Fig.3. Crystal growth and coarsening mechanisms in magnesium alloys based on in situ 4D synchrotron radiation imaging technique (a-d) crystal coarsening behaviors of Mg-Zn alloy during isothermal holding[30] (Insets in Figs.3c and d are enlarged views) (e-h) 3D crystal growth in Mg-25%Zn-7%Al alloy (e, f) and Mg-25%Zn-7%Al composites with 0.7%SiC nano ceramic particles (g, h)[36] (NP—nanoparticle, Tl—melt temperature, —cooling rate, fs—solid fraction)
|
|
 |
|
|