[an error occurred while processing this directive]
基于同步辐射原位表征技术的镁合金研究进展
郭恩宇1,2(), 杜泽龙1, 李炳志1, 王同敏1,2()
Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques
GUO Enyu1,2(), DU Zelong1, LI Bingzhi1, WANG Tongmin1,2()

图2. 电磁场作用下基于同步辐射光源的凝固行为实时成像装置示意图[17,18]和照片及多功能/多环境服役原位加载装置

Fig.2. Real-time imaging device for electro-magnetic solidification behavior based on synchrotron radiation source and multi-functional/multi-environment service in situ loading device
(a, b) schematic (a)[17,18] and on-site photo (b) of the solidification device integrating electromagnetic fields (CCD—charge coupled device, DC—direct current)
(c) in situ high temperature vacuum solidification furnace at Shanghai Synchrotron Radiation Facility (SSRF)
(d) in situ 4D high temperaturesolidification furnace at SSRF
(e) physical diagram of the in situ 4D loading device developed based on the imaging line station at SSRF
(f) schematic showing the structure of a mechanical rig for in situ microdiffraction experiment at SSRF