单晶高温合金近服役环境下的变形损伤行为
|
|
Deformation and Damage Behavior of Single Crystal Superalloys Under Near-Service Conditions
|
|
图3. 单晶高温合金热机械疲劳(TMF)变形机制示意图 |
Fig.3. Schematics of the thermal-mechanical fatigue (TMF) deformation mechanism in single-crystal superalloys (OP—out-of-phase, IP—in-phase) |
![]() |