图2. 不同加载条件下单晶高温合金的疲劳裂纹萌生机制

Fig.2. Fatigue crack initiation mechanism under different loading conditions
(a) cracking of carbides is attributed to the combination of oxidizing and cyclic loading
(b) crack initiating from slip band shearing around casting pore
(c) γ′-rotation within the rough zone around casting pore is related to the operation of {111}<110> and {111}<112> slip systems (σ—stress)
(d) slip bands with different direction observed within eutectic show more uniform deformation
(e) hot isostatic pressing (HIP) specimens mainly fail from the surface oxidation and present the best fatigue property