异种材料连接技术及其在复杂结构制造中的应用
冯吉才, 宋晓国, 刘多, 周利, 檀财旺, 陈波

Joining Technology of Dissimilar Materials and Its Application in Complex Structure Manufacturing
FENG Jicai, SONG Xiaoguo, LIU Duo, ZHOU Li, TAN Caiwang, CHEN Bo
表1 钎焊接头应力调控方法的优势与局限[3]
Table 1 Advantages and limitations of stress control methods of brazed joints[3]
Stress regulation method

Advantage

Limitation

Composite brazing filler

(1) Flexibly control the thermal expansion coefficient of the solder to reduce the mismatch of the thermal expansion coefficient;

(2) The fine nucleation particles formed by itself or reaction can disperse and strengthen the brazing seam;

(3) Inhibit element diffusion and reduce the formation of large intermetallic compounds

(1) It affects the fluidity of the solder and is prone to causing void defects;

(2) The reinforcing phase is prone to agglo-meration and is likely to cause defects in the joint

Middle layer

(1) Simple and efficient, reducing stress concentration;

(2) It serves as a barrier layer, regulates interfacial reactions, and inhibits element diffusion;

(3) The porous intermediate layer can refine the microstructure of the brazed seam and improve its plasticity and toughness

(1) Limited by the lamellar structure;

(2) It may cause a decrease in the assembly accuracy of the joint;

(3) The processing technology of the composite intermediate layer is complex

Surface structure design

(1) Effectively increase the connection area;

(2) Change the distribution state of residual stress to form a gradient transition;

(3) For the stress concentration area, improve the crack fracture path and form a pinning strengthening effect

(1) Low processing efficiency;

(2) It is prone to causing damage to the base material