异种材料连接技术及其在复杂结构制造中的应用
|
冯吉才 1,2, 宋晓国 1,2(  ), 刘多 2, 周利 2, 檀财旺 2, 陈波 2
|
|
Joining Technology of Dissimilar Materials and Its Application in Complex Structure Manufacturing
|
FENG Jicai 1,2, SONG Xiaoguo 1,2(  ), LIU Duo 2, ZHOU Li 2, TAN Caiwang 2, CHEN Bo 2
|
|
|
图7. 激光改性Si3N4陶瓷获得的Si/Si3N4界面TEM分析结果[68]
|
Fig.7. TEM analysis results from the Si/Si3N4 interface of the Si3N4 ceramic after laser modification[68] (a) BF-TEM image (b-d) SAED pattern (b), HETEM image and SAED pattern (inset) (c), and IFFT image (d) taken in marked A1 in Fig.7a (d—interplanar spacing) (e-g) SAED pattern (e), HETEM image and SAED pattern (inset) (f), and IFFT image (g) taken in marked A2 in Fig.7a (h, i) HRTEM images and SAED patterns (insets) taken in marked A3 in Fig.7a
|
|
 |
|
|