图5. 三种成分梯度20%、10%、5%沉积形式及沿沉积方向的平均一次枝晶臂间距变化,20%梯度材料的XRD谱,及三种梯度断裂面形貌[ |
Fig.5. Three composition gradient deposition forms of 20% (component A), 10% (component B), and 5% (component C) (a), variations of average primary dendritic arm spacing (PDAS) along the deposition direction (b), XRD patterns at different location obtained for component A (c), and fracture surfaces of the three gradient specimens (d)[ |
![]() |