异种材料连接技术及其在复杂结构制造中的应用
|
|
Joining Technology of Dissimilar Materials and Its Application in Complex Structure Manufacturing
|
|
图4. 四种改性类型的TC4/CFRTP局部横截面形貌分析[ |
Fig.4. Local cross-sectional topography analyses (including OM images, SEM images, and EDS elements distribution) of TC4/CFRTP with four modified types (CFRTP—carbon fiber reinforced thermal plastic) [ |
![]() |