[an error occurred while processing this directive]
矩张量机器学习势模型的发展与应用
陈星秋1(), 王建韬1,2, 刘培涛1()
Moment Tensor Machine-Learning Potential: Development and Applications
CHEN Xing-Qiu1(), WANG Jiantao1,2, LIU Peitao1()

图6. MTP模型在QM9数据集上的主动学习与随机选择策略的效率和性能比较[64]

Fig.6. Efficiency and property comparisons of active learning vs random sampling for training a MTP model on the QM9 dataset[64] (a, b) root-mean-square (RMS) error (a) and maximal error (b) as a function of training set size (c) parity plot of MTP-predicted enthalpy (HMT) vs reference enthalpy (Href) for a model trained with random selection (d) parity plot for a model trained with active learning