难加工金属增材制造/热等静压融合成形研究现状与展望
史玉升, 程焜, 张程健, 卢佳浩, 李伟, 张李超, 魏青松, 蔡超

Research Status and Prospects of Additive Manufacturing/Hot Isostatic Pressing Integrated Forming for Difficult-to-Machine Metals
SHI Yusheng, CHENG Kun, ZHANG Chengjian, LU Jiahao, LI Wei, ZHANG Lichao, WEI Qingsong, CAI Chao
表1 典型难加工材料的性能优势、加工难点以及应用场景[29~44]
Table 1 Advantageous performances, process characteristics, and applications of typical difficult-to-machine materials[29~44]
Material categoryGrade or compositionAdvantageous performanceDifficult to process characteristicsApplication

Be and Be alloy

S-200F[29]

(Be ≥ 98.5%),

AlBeMet 162[30]

(Be-38Al)

(1) Specific stiffness: 86-164 GPa·cm3·g-1

(2) Thermal conductivity:210-220 W·m-1·K-1

(3) Coefficient of thermal expansion: (11.5-13.9) × 10-6 K-1

(4) Infrared reflectance: 98%-99%

(1) Low ductility and prone to cracking during casting

(2) High intrinsic brittleness and prone to cracking during machining

(3) Highly toxic and constrained in supply; fully enclosed processing and strict protection are required, leading to high cost and limited capacity

(1) Aerospace field: inertial navigation platforms, gyro components, and lightweight load bearing structures with high stiffness

(2) Optics and semiconductor equipment field: metal mirrors for infrared and astronomical telescopes, EUV lithography mirror substrates

(3) Nuclear and extreme thermal environments: first wall or plasma facing materials for fusion devices and high heat flux thermal management components

Ti2AlNb alloy

Ti-22Al-25Nb[31],

Ti-45Al-5Nb-0.3 W[32],

Ti-22Al-25Nb[33],

Ti2AlNb[34]

(1) Ultimate tensile strength: 880-937 MPa at 650 oC

(2) Elongation: 137%-167% at 900 oC

(3) Fatigue limit: 400-470 MPa at 650-700 oC, 107 cyc

(4) Creep life: 201 h (550 oC, 600 MPa)

(1) Severe cracking is commonly observed during rapid solidification

(2) Process control is challenging, resulting in frequent internal defects in formed parts

(1) Aeroengine field: multiple key components such as aeroengine forgings and blade billets

(2) Medical field: orthopedic hard tissue repair devices such as artificial joints, spinal fusion cages, and bone plates

Ni based superalloy with high Ti and Al contents

CMSX-4[37,40],

IN738LC[35],

CM247LC[36],

Mar-M247[38,39]

(1) Ultimate tensile strength: 1050-1150 MPa at 750 oC

(2) Elongation: 45.5%-55.4% at 900 oC

(3) High temperature fatigue limit: 280-320 MPa at 750 oC, 107 cyc

(4) Creep life: 320 h at 800 oC, 250 MPa

(1) Wide solidification range; the interdendritic liquid film readily induces hot tearing

(2) High thermal gradients and rapid cooling generate significant residual stress and cause cracking

(3) Process control is difficult, making it hard to obtain the desired microstructure directly

(1) Aeroengine field: standard material for high pressure turbine of 4th and 5th generation high thrust turbofan engines, also used for combustors, guide vanes, and related parts

(2) Domestic aero power field: “Taihang” series military turbofan engines

(3) Energy field: suitable for supercritical power plant boiler superheaters

Metal matrix composites

55%*SiC/Al[41],

60%*diamond/Cu[42],

65%*SiC/Cu[43],

30%*B4C/Al[44]

(1) Coefficient of thermal expansion: (6-15.8) × 10-6 K-1

(2) Thermal conductivity: 400-900 W·m-1·K-1

(3) Elastic modulus: 180-472 GPa at RT

(1) Large thermal expansion mismatch between ceramic reinforcement and metal matrix; solidification easily produces thermal stress and induces cracking or porosity

(2) High ceramic fraction leads to brittleness and poor plasticity; severe tool wear during machining and frequent tool chipping

(1) Aerospace field: load bearing and frequently disassembled parts such as aircraft ventral fin skins, fuel inlet covers, internal guide rails, and angle stiffeners

(2) Precision instruments field: load bearing components such as gimbals, brackets, and instrument bay sections for strategic missile systems, as well as laser gyro cavities and optical support structures

(3) Thermal management field: housings and bases for radar T/R modules, baseplates for IGBT power modules, and thin wall packages for optoelectronic and optical communication devices