[an error occurred while processing this directive]
综述:定向凝固枝晶生长的数值模拟
董洪标1(), 郝文硕2
Numerical Modeling of Dendrite Growth During Directional Solidification: A Review
DONG Hongbiao1(), HAO Wenshuo2

图4. 利用高速凝固法(恒定抽拉速率3 mm/min)和液态金属冷却法(恒定抽拉速率8 mm/min)制备单晶叶片时的温度场和糊状区演变[18]

Fig.4. Temperature fields and mushy zone evolutions during single-crystal blade fabrication by high rate solidification at a constant withdrawal rate of 3 mm/min (a1-a5) and liquid metal cooling at a constant withdrawal rate of 8 mm/min (b1-b5)[18]
(a1) t = 241 s, fs = 30% (t—solidification time, fs—solid volume fraction)
(a2) t = 2028 s, fs = 40% (a3) t = 2411 s, fs = 50%
(a4) t = 2632 s, fs = 60% (a5) t = 2987 s, fs = 80%
(b1) t = 205 s, fs = 30% (b2) t = 689 s, fs = 40%
(b3) t = 910 s, fs = 50% (b4) t = 1031 s, fs = 60%
(b5) t = 1193 s, fs = 80%