[an error occurred while processing this directive]
综述:定向凝固枝晶生长的数值模拟
董洪标1(), 郝文硕2
Numerical Modeling of Dendrite Growth During Directional Solidification: A Review
DONG Hongbiao1(), HAO Wenshuo2

图1. 凝固前沿固/液界面处的溶质浓度分布和成分过冷区

Fig.1. Solute concentration at the solidification front (solid/liquid interface) (a) and constitutional undercooling zone indicated by the shadow region (b) (C—compositon; CS, CL, and C∞—compositions of solid, liquid, and alloys, respectively. Z—distance from solid/liquid interface. T—temperature, T(CL)—equilibrium liquidus temperature at the solidification front, T(C∞)—equilibrium liquidus temperature corresponding to C∞. G—applied thermal gradient, GTL—thermal gradient of equilibrium liquidus temperature)