[an error occurred while processing this directive]
面向极端服役条件的高熵合金结构材料:性能优势、瓶颈与突破路径
吕昭平(), 申耀祖, 王先珍, 陈强, 唐建国, 张晓宾, 于勇, 蒋虽合, 刘雄军, 王辉, 吴渊
High-Entropy Alloys in Extreme Environments: A Perspective on Advantages, Challenges, and Breakthroughs
LU Zhaoping(), SHEN Yaozu, WANG Xianzhen, CHEN Qiang, TANG Jianguo, ZHANG Xiaobin, YU Yong, JIANG Suihe, LIU Xiongjun, WANG Hui, WU Yuan

图7. 局域化学有序结构和成分波动对高熵合金中辐照缺陷的影响[74]

Fig.7. More pronounced chemical short-range order (CSRO) (a) and chemical fluctuation (b) in NiCoCrFeMn-CN compared to NiCoCrFeMn suppress void swelling (c, d) showing the influence of local chemical ordered structures and compositional fluctuations on irradiation defects in HEAs[74] (D, Dvac, and Dinter represent the diffusion coefficient, diffusion coefficient of self-interstitial atoms, and diffusion coefficient of vacancies, respectively)