面向极端服役条件的高熵合金结构材料:性能优势、瓶颈与突破路径
吕昭平(), 申耀祖, 王先珍, 陈强, 唐建国, 张晓宾, 于勇, 蒋虽合, 刘雄军, 王辉, 吴渊
High-Entropy Alloys in Extreme Environments: A Perspective on Advantages, Challenges, and Breakthroughs
LU Zhaoping(), SHEN Yaozu, WANG Xianzhen, CHEN Qiang, TANG Jianguo, ZHANG Xiaobin, YU Yong, JIANG Suihe, LIU Xiongjun, WANG Hui, WU Yuan

图6. 主元数量对合金中空洞等辐照缺陷的影响[65]

Fig.6. Cross-sectional TEM images of Ni, NiFe, NiCoFe, and NiCoFeCrMn irradiated with 3 MeV Ni+ to 5 × 1016 cm-2 at 773 K showing the influence of the number of principal elements on irradiation defects in alloys[65]