跨尺度协同增强铝基复合材料研究进展
欧阳求保, 苏楠, 王瑞安, 刘侃, 张荻()
Research Progress on Cross-Scale Synergistically Reinforced Aluminum Matrix Composites
OUYANG Qiubao, SU Nan, WANG Ruian, LIU Kan, ZHANG Di()

图1. 原位自生SiC颗粒(SiCp)碳纳米管(CNTs)增强铝基复合材料制备流程示意图[2]

Fig.1. Schematics of the preparation process of in situ self-generated SiC particles (SiCp) carbon nanotubes (CNTs)-reinforced aluminium matrix composites[2] (CVD—chemical vapor deposition)