[an error occurred while processing this directive]
TiAl合金疲劳小裂纹行为
相恒高1,2,3, 宋伟东1,2,3, 加陆毅1,2,3, 祁志祥1,2,3, 陈旸1,2,3(), 周冰1,2,3, 郑功1,2,3, 应盼1,2,3, 陈光1,2,3
Fatigue Small Crack Behavior of TiAl Alloys
XIANG Henggao1,2,3, Song Weidong1,2,3, JIA Luyi1,2,3, QI Zhixiang1,2,3, CHEN Yang1,2,3(), ZHOU Bing1,2,3, ZHENG Gong1,2,3, YING Pan1,2,3, CHEN Guang1,2,3

图5. Ti-45Al-5Nb-0.2C-0.2B合金中不同片层取向下小裂纹萌生位置的数量[34]

Fig.5. Relative numbers of small crack initiation sites in Ti-45Al-5Nb-0.2C-0.2B alloy under different lamellar orientations (θ)[34]