[an error occurred while processing this directive]
TiAl合金疲劳小裂纹行为
相恒高1,2,3, 宋伟东1,2,3, 加陆毅1,2,3, 祁志祥1,2,3, 陈旸1,2,3(), 周冰1,2,3, 郑功1,2,3, 应盼1,2,3, 陈光1,2,3
Fatigue Small Crack Behavior of TiAl Alloys
XIANG Henggao1,2,3, Song Weidong1,2,3, JIA Luyi1,2,3, QI Zhixiang1,2,3, CHEN Yang1,2,3(), ZHOU Bing1,2,3, ZHENG Gong1,2,3, YING Pan1,2,3, CHEN Guang1,2,3

图3. Ti-46Al-4Nb-1.8Cr-0.2Ta合金中疲劳小裂纹在片层团界处萌生及扩展的示意图[37]

Fig.3. Schematic of initiation and propagation of fatigue small cracks in Ti-46Al-4Nb-1.8Cr-0.2Ta alloy at the interface of lamellar colony[37]