TiAl合金疲劳小裂纹行为
|
相恒高 1,2,3, 宋伟东 1,2,3, 加陆毅 1,2,3, 祁志祥 1,2,3, 陈旸 1,2,3(  ), 周冰 1,2,3, 郑功 1,2,3, 应盼 1,2,3, 陈光 1,2,3
|
|
Fatigue Small Crack Behavior of TiAl Alloys
|
XIANG Henggao 1,2,3, Song Weidong 1,2,3, JIA Luyi 1,2,3, QI Zhixiang 1,2,3, CHEN Yang 1,2,3(  ), ZHOU Bing 1,2,3, ZHENG Gong 1,2,3, YING Pan 1,2,3, CHEN Guang 1,2,3
|
|
|
图1. 小裂纹和长裂纹的疲劳裂纹扩展速率[10]
|
Fig.1. Fatigue crack propagation rates of small and long cracks[10] (a—crack length, N—number of cycles, ΔK—stress intensity factor range)
|
|
 |
|
|