[an error occurred while processing this directive]
金属材料晶界结构的拓扑性质与表征
朱思瑛(), 易敏, 郭万林()
Topological Properties and Characteristics of Grain Boundary Structure in Metallic Materials
ZHU Siying(), YI Min, GUO Wanlin()

图8. 3D晶界网络与离散胞复形的映射关系,不同大塑性变形(SPD)工艺处理的演化范围[1],3D晶界网络的连续动态再结晶(CDRX)演化过程示意图,及Betti数在有限元(FEM)样品中的分布[153]

Fig.8. Mapping relationship between 3D grain boundary network and discrete cell complex structure (a)[1], evolution ranges under different SPDs (SPD—severe plastic deformation, HAGBs—high angle grain boundaries, ARB—accumulative roll bonding, HPT—high-pressure torsion, ECAP—equal-channel angular pressing) (b)[1], schematics of 3D grain boundary network evolution during CDRX (LAGB—low angle grain boundary) (c)[153], and Betti number distributions through finite element method (FEM) sample (d)[153]