Fig.6. Topological grain boundary dislocation network transformations in {210}[0001] orientation[114] (a) adding Ti atoms (light blue) to the left half of the ground-state structure and performing high-temperature molecular dynamics simulations trigger a dislocation-pairing transformation in a quasi-2D geometry. The top panels clearly show how the green dislocation lines pair up to form purple ones. The gray atoms are hcp coordinated, while red and dark blue atoms highlight different dislocation core structures (b) analogously, adding Ti atoms (dark red) to the left half of the metastable structure triggers a dislocation-unpairing transition locally (c) topological transition of the grain boundary dislocation network upon defect absorption. The view of the grain boundary plane shows a paired-dislocation grain boundary island (nucleus in purple) inside the parent ground state (green dislocation lines)
|