金属材料晶界结构的拓扑性质与表征
朱思瑛(), 易敏, 郭万林()
Topological Properties and Characteristics of Grain Boundary Structure in Metallic Materials
ZHU Siying(), YI Min, GUO Wanlin()

图4. 通过蓝色立方晶格绕垂直于纸面的[001]轴旋转获得的共格点阵构型(重合点阵密度倒数Σ ≤ 25)[3],Σ3和Σ9晶界、Σ3晶界在应变驱动下的演化和Σ3 n 相互作用示意图[104]

Fig.4. Σ25 at 16° (a1), Σ13 at 22° (a2), Σ17 at 28° (a3), and Σ5 at 36° (a4) coincident site lattice configurations (reciprocal of coincidence site lattice (CSL) density Σ ≤ 25) obtained by rotations of the blue cubic lattice about a common [001] axis normal to the plane of the paper[3] (Black lines indicate the CSL repeat units); schematics of Σ3 (b1) and Σ9 (b2) boundaries, strain-driven evolution of a Σ3 boundary (b3), and Σ3 n interaction (b4)[104]