生物可降解纯Mg表面BA + Alg@Ca复合涂层的制备及其体外生物相容性 |
| 梁涛, 杜云波, 陈协辉, 潘浩波 |
|
Fabrication and in vitro Biocompatibility Evaluation of BA + Alg@Ca Composite Coatings on Biodegradable Pure Mg |
| LIANG Tao, DU Yunbo, CHEN Xiehui, PAN Haobo |
| 图3 BA样品的抗菌性能 |
| Fig.3 Antibacterial properties of control, untreated, and BA samples against Staphylococcus aureus (S. aureus), Escherichia coli (E. coli), and Acinetobacterbaumannii (A. baumannii) (Ti6Al4V titanium alloy was used as control sample, the same below) |
|