生物可降解纯Mg表面BA + Alg@Ca复合涂层的制备及其体外生物相容性 |
| 梁涛, 杜云波, 陈协辉, 潘浩波 |
|
Fabrication and in vitro Biocompatibility Evaluation of BA + Alg@Ca Composite Coatings on Biodegradable Pure Mg |
| LIANG Tao, DU Yunbo, CHEN Xiehui, PAN Haobo |
| 图2 对纯Mg进行不同浓度H3BO3水热溶液处理所得BA样品的电化学测试结果 |
| Fig.2 Open circuit potential (OCP) curves (a), Nyquist plots (b), and potential dynamic curves (c) of BA samples (SCE—saturated calomel electrode, ZRe—real part of impedance, ZIm—imaginary part of impedance) |
|