耐腐蚀磨损CrN/NbN涂层的沉积机制及缺陷控制
|
|
刘永康, 陆媛媛, 杨英, 刘兴光, 郑军, 张世宏
|
Deposition Mechanism and Defect Control of CrN/NbN Coatings with Excellent Tribocorrosion Performance
|
|
LIU Yongkang, LU Yuanyuan, YANG Ying, LIU Xingguang, ZHENG Jun, ZHANG Shihong
|
|
表2 S1~S6涂层样品在3.5%NaCl溶液中的EIS拟合结果
|
Table 2 EIS fitting results of S1-S6 coating samples in 3.5%NaCl solution
|
|
| Coating | Rs | Q1 | Rpo | Q2 | Rct |
|---|
| Ω·cm2 | Ω·cm2 | Ω·cm2 |
|---|
Ypo Ω-1·cm-2·S n | n1 | Yct Ω-1·cm-2·S n | n2 |
|---|
| | | | | S1 | 29.26 | 5.53 × 10-5 | 0.8865 | 3.53 × 102 | 1.11 × 10-4 | 0.7290 | 1.04 × 104 | | S2 | 31.47 | 2.88 × 10-5 | 0.9184 | 1.03 × 103 | 3.95 × 10-5 | 0.5009 | 5.58 × 104 | | S3 | 31.51 | 2.07 × 10-5 | 0.9410 | 4.22 × 103 | 4.22 × 10-5 | 0.5595 | 7.07 × 104 | | S4 | 27.08 | 1.57 × 10-5 | 0.8756 | 1.03 × 103 | 3.30 × 10-5 | 0.4490 | 2.88 × 105 | | S5 | 25.55 | 1.28 × 10-5 | 0.8817 | 3.58 × 103 | 5.01 × 10-5 | 0.5238 | 6.19 × 105 | | S6 | 28.18 | 2.58 × 10-5 | 0.8858 | 4.03 × 103 | 2.26 × 10-5 | 0.5387 | 1.38 × 105 |
|
|
|