耐腐蚀磨损CrN/NbN涂层的沉积机制及缺陷控制
刘永康, 陆媛媛, 杨英, 刘兴光, 郑军, 张世宏

Deposition Mechanism and Defect Control of CrN/NbN Coatings with Excellent Tribocorrosion Performance
LIU Yongkang, LU Yuanyuan, YANG Ying, LIU Xingguang, ZHENG Jun, ZHANG Shihong
图21 涂层腐蚀磨损机理示意图
Fig.21 Schematics of tribocorrosion mechanism of different coatings
(a) single-layer coating
(b) multilayer/nanomultilayer coating
(c) multilayer/nanomultilayer coating + ion etching