耐腐蚀磨损CrN/NbN涂层的沉积机制及缺陷控制
刘永康, 陆媛媛, 杨英, 刘兴光, 郑军, 张世宏

Deposition Mechanism and Defect Control of CrN/NbN Coatings with Excellent Tribocorrosion Performance
LIU Yongkang, LU Yuanyuan, YANG Ying, LIU Xingguang, ZHENG Jun, ZHANG Shihong
图19 S2涂层样品磨痕截面形貌的SEM像
Fig.19 Low (a) and high (b, c) magnified SEM images of wear track cross-section in S2 coating sample