耐腐蚀磨损CrN/NbN涂层的沉积机制及缺陷控制 |
| 刘永康, 陆媛媛, 杨英, 刘兴光, 郑军, 张世宏 |
|
Deposition Mechanism and Defect Control of CrN/NbN Coatings with Excellent Tribocorrosion Performance |
| LIU Yongkang, LU Yuanyuan, YANG Ying, LIU Xingguang, ZHENG Jun, ZHANG Shihong |
| 图13 S1~S6涂层样品在3.5%NaCl (质量分数)溶液中的电化学阻抗谱(EIS)和等效电路 |
| Fig.13 Electrochemical impedance spectroscopies (EIS) (a-c) and equivalent circuit (d) of S1-S6 coating samples in 3.5%NaCl solution (a) Nyquist plots (Inset is the partially enlarged view, Zim—imaginary part of impedance, Zre—real part of impedance) (b) Bode impedance magnitude plots (Inset is the partially enlarged view, |Z|—modulus of impedance, f—frequency) (c) Bode phase angle plots (d) modeled equivalent circuit (Rs—solution resistance, Q1 and Q2—constant phase elements, Rpo—coating pore resistance, Rct—charge transfer resistance, RE—reference electrode, WE—working electrode) |
|