耐腐蚀磨损CrN/NbN涂层的沉积机制及缺陷控制 |
| 刘永康, 陆媛媛, 杨英, 刘兴光, 郑军, 张世宏 |
|
Deposition Mechanism and Defect Control of CrN/NbN Coatings with Excellent Tribocorrosion Performance |
| LIU Yongkang, LU Yuanyuan, YANG Ying, LIU Xingguang, ZHENG Jun, ZHANG Shihong |
| 图1 镀膜设备及沉积过程示意图 |
| Fig.1 Schematics of coating equipment and deposition process (Nos.1-4 are the metal targets, S1-S6 represents coatings with different preparation processes) |
|