表层多孔Ti6Al4V/TiC梯度材料的构筑、组织和性能
邵星海, 王文焱, 谢敬佩, 秦文栋, 王爱琴, 马窦琴, 毛志平, 柳培, 郭清远

Construction, Microstructure, and Properties of Ti6Al4V/TiC Functionally Graded Material with Porous Surface
SHAO Xinghai, WANG Wenyan, XIE Jingpei, QIN Wendong, WANG Aiqin, MA Douqin, MAO Zhiping, LIU Pei, GUO Qingyuan
图12 钛层、Ti-4%TiC层、Ti-6%TiC层和Ti-8%TiC层的抗拉强度和断后伸长率
Fig.12 Tensile strengths and elongations after fracture of titanium layer, Ti-4%TiC layer, Ti-6%TiC layer, and Ti-8%TiC layer