表层多孔Ti6Al4V/TiC梯度材料的构筑、组织和性能 |
| 邵星海, 王文焱, 谢敬佩, 秦文栋, 王爱琴, 马窦琴, 毛志平, 柳培, 郭清远 |
|
Construction, Microstructure, and Properties of Ti6Al4V/TiC Functionally Graded Material with Porous Surface |
| SHAO Xinghai, WANG Wenyan, XIE Jingpei, QIN Wendong, WANG Aiqin, MA Douqin, MAO Zhiping, LIU Pei, GUO Qingyuan |
| 图2 试样制备示意图 |
| Fig.2 Schematic of sample preparation |
|