Spatial Distribution and Evolution Mechanism of Texture in Non-Oriented Silicon Steel Influenced by the Grain Boundary Segregation Element Sb
CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang
表2 无取向硅钢板在晶粒长大退火后的磁性能
Table 2 Magnetic properties of non-oriented silicon steel sheets after grain growth annealing
SampleB50 / TP15/50 / (W·kg-1)
RDTDRDTD
0Sb1.671.633.143.25
4Sb1.711.663.033.18