晶界偏聚元素Sb作用下无取向硅钢织构的空间分布与演变机制 |
| 常松涛, 张芳, 沙玉辉, 左良 |
|
Spatial Distribution and Evolution Mechanism of Texture in Non-Oriented Silicon Steel Influenced by the Grain Boundary Segregation Element Sb |
| CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang |
| 图9 晶界偏聚元素干预无取向硅钢再结晶织构竞争的示意图 |
| Fig.9 Schematics of recrystallization texture competition mediated by segregation elements in non-oriented silicon steel sheets without (a, c, e, g) and with (b, d, f, h) Sb addition (a, b) early recrystallization stage (c, d) middle recrystallization stage (e, f) complete recrystallization (g, h) after grain growth |
|