晶界偏聚元素Sb作用下无取向硅钢织构的空间分布与演变机制 |
| 常松涛, 张芳, 沙玉辉, 左良 |
|
Spatial Distribution and Evolution Mechanism of Texture in Non-Oriented Silicon Steel Influenced by the Grain Boundary Segregation Element Sb |
| CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang |
| 图8 初次再结晶组织结构示意图和平均晶粒尺寸随退火时间的演变 |
| Fig.8 Schematic of primary recrystallization microstructure (a) and the evolution of average grain size during grain growth (b) |
|