晶界偏聚元素Sb作用下无取向硅钢织构的空间分布与演变机制 |
| 常松涛, 张芳, 沙玉辉, 左良 |
|
Spatial Distribution and Evolution Mechanism of Texture in Non-Oriented Silicon Steel Influenced by the Grain Boundary Segregation Element Sb |
| CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang |
| 图4 无Sb和含Sb初次再结晶和晶粒长大无取向硅钢板主要织构组分的面积分数 |
| Fig.4 Area fractions of major texture components in non-oriented silicon steel sheets without (a) and with (b) Sb addition after primary recrystallization and grain growth |
|