晶界偏聚元素Sb作用下无取向硅钢织构的空间分布与演变机制
常松涛, 张芳, 沙玉辉, 左良

Spatial Distribution and Evolution Mechanism of Texture in Non-Oriented Silicon Steel Influenced by the Grain Boundary Segregation Element Sb
CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang
图3 无Sb和含Sb初次再结晶和晶粒长大无取向硅钢板取向分布函数(ODF)的φ2 = 0°和45°截面图 (φ2为Euler角)
Fig.3 Constant φ2 = 0° and 45° sections of ODFs of non-oriented silicon steel sheets without (a, c) and with (b, d) Sb addition after primary recrystallization (a, b) and grain growth (c, d) (ODF—orientation distribution function; φ1, φ2, and Φ—Euler angles)