稀土合金化石油套管钢精炼-连铸-轧制过程夹杂物演变行为 |
| 梁雨雨, 倪培远, 刘麒麟, 厉英 |
|
Evolution Behavior of Inclusions in Rare Earth Metal Alloying Oil Casing Steel During Refining and Casting and Hot-Rolling Process |
| LIANG Yuyu, NI Peiyuan, LIU Qilin, LI Ying |
| 图15 不加稀土炉次和加稀土炉次热轧管坯样不同Ca含量夹杂物的SEM像和EDS分析 |
| Fig.15 SEM images showing the deformation behaviors of inclusions with different Ca contents and EDS analysis of hot rolled tube blank in RE-free steel and RE steel (a1-a3) RE-free steel with low Ca content (< 12%), along RD (a1), TD (a2), and ND (a3) (b1-b3) RE-free steel with medium Ca content (12%-21%), along RD (b1), TD (b2), and ND (b3) (c1-c3) RE-free steel with high Ca content (> 21%), along RD (c1), TD (c2), and ND (c3) (d1-d3) RE steel with no Ca content limit, along RD (d1), TD (d2), and ND (d3) |
|