稀土合金化石油套管钢精炼-连铸-轧制过程夹杂物演变行为 |
| 梁雨雨, 倪培远, 刘麒麟, 厉英 |
|
Evolution Behavior of Inclusions in Rare Earth Metal Alloying Oil Casing Steel During Refining and Casting and Hot-Rolling Process |
| LIANG Yuyu, NI Peiyuan, LIU Qilin, LI Ying |
| 图7 精炼及连铸过程夹杂物种类分布示意图 |
| Fig.7 Schematics of the distribution of inclusion type in refining and continuous casting process (a) R1 (b) RF2 (c) R3 (d) R4 (e) R5 (f) RF5 |
|