稀土合金化石油套管钢精炼-连铸-轧制过程夹杂物演变行为 |
| 梁雨雨, 倪培远, 刘麒麟, 厉英 |
|
Evolution Behavior of Inclusions in Rare Earth Metal Alloying Oil Casing Steel During Refining and Casting and Hot-Rolling Process |
| LIANG Yuyu, NI Peiyuan, LIU Qilin, LI Ying |
| 图6 加稀土炉次铸坯样中典型夹杂物形貌的SEM像、EDS分析结果和形貌示意图 |
| Fig.6 Typical SEM images, EDS analysis results, and schematics of morphology of inclusions in RE steel casting billet sample (a-d) SEM images and corresponding EDS point scanning results (e-h) SEM images and corresponding EDS element mapping analyses of square regions, and corresponding schematics of inclusion morphologies |
|