低碳低合金钢焊缝熔覆金属针状铁素体的回火稳定性 |
| 胡富昇, 成林, 侯廷平, 程石, 宋峰雨, 吴开明 |
|
High-Temperature Stability of Acicular Ferrite in a Low-Carbon Low-Alloy Steel Weld Metal |
| HU Fusheng, CHENG Lin, HOU Tingping, CHENG Shi, SONG Fengyu, WU Kaiming |
| 图9 焊缝熔敷金属在焊态及不同温度和时间回火后的硬度、抗拉强度、伸长率及冲击吸收功 |
| Fig.9 Hardnesses (a), tensile strengths (b), elongations (c), and impact absorbing energies (d) of weld metal specimens at as-welded state and tempering at different temperatures and time |
|