回火温度对超深井承压件F22M钢微观组织与力学性能的影响 |
| 江慧敏, 魏梦洁, 胡小强, 蔡欣, 李殿中, 党恩 |
|
Effects of Tempering Temperature on the Microstructure and Mechanical Properties of F22M Steel for Blowout Preventer in Ultra-Deep Well |
| JIANG Huimin, WEI Mengjie, HU Xiaoqiang, CAI Xin, LI Dianzhong, DANG En |
| 图11 回火态F22M钢屈服强度的计算值与实验值对比 |
| Fig.11 Comparisons of experimental and theoretical yield strengths of F22M steel with different tempering temperatures (σdis + ppt—dislocation and precipitation strengthening, σgb—grain refinement strengthening, σs—solid solution strengthening, σ0—lattice friction stress) |
|