回火温度对超深井承压件F22M钢微观组织与力学性能的影响 |
| 江慧敏, 魏梦洁, 胡小强, 蔡欣, 李殿中, 党恩 |
|
Effects of Tempering Temperature on the Microstructure and Mechanical Properties of F22M Steel for Blowout Preventer in Ultra-Deep Well |
| JIANG Huimin, WEI Mengjie, HU Xiaoqiang, CAI Xin, LI Dianzhong, DANG En |
| 图10 热力学平衡状态F22M钢中析出相质量分数随温度的变化曲线 |
| Fig.10 Mass fraction variations of carbides in F22M steel with the equilibrium state among the temperature from 400 oC to 900 oC |
|