回火温度对超深井承压件F22M钢微观组织与力学性能的影响 |
| 江慧敏, 魏梦洁, 胡小强, 蔡欣, 李殿中, 党恩 |
|
Effects of Tempering Temperature on the Microstructure and Mechanical Properties of F22M Steel for Blowout Preventer in Ultra-Deep Well |
| JIANG Huimin, WEI Mengjie, HU Xiaoqiang, CAI Xin, LI Dianzhong, DANG En |
| 图8 不同回火温度后F22M钢的-29 ℃冲击功 |
| Fig.8 Impact absorbed energies at -29 oC of F22M steel with different tempering temperatures |
|