回火温度对超深井承压件F22M钢微观组织与力学性能的影响
江慧敏, 魏梦洁, 胡小强, 蔡欣, 李殿中, 党恩

Effects of Tempering Temperature on the Microstructure and Mechanical Properties of F22M Steel for Blowout Preventer in Ultra-Deep Well
JIANG Huimin, WEI Mengjie, HU Xiaoqiang, CAI Xin, LI Dianzhong, DANG En
图3 610 ℃回火后F22M钢微观组织的SEM像和TEM分析
Fig.3 SEM image (a) and TEM analyses (b-h) of F22M steel tempered at 610 oC (Insets in Figs.3b and c show the corresponding fast Fourier transform (FFT) patterns of the rectangle areas; inset in Fig.3d shows the corresponding selected area electron diffraction (SAED) pattern of the rectangle area) (b-d) TEM images of M3C (b) and M7C3 (c, d) carbides (e, f) EDS analyses of M3C (e) and M7C3 (f) carbides (g, h) TEM image of the tiny ellipsoidal carbides precipitated in the bainitic ferrite matrix (g) and corresponding EDS elemental distribution mappings (h)