回火温度对超深井承压件F22M钢微观组织与力学性能的影响 |
| 江慧敏, 魏梦洁, 胡小强, 蔡欣, 李殿中, 党恩 |
|
Effects of Tempering Temperature on the Microstructure and Mechanical Properties of F22M Steel for Blowout Preventer in Ultra-Deep Well |
| JIANG Huimin, WEI Mengjie, HU Xiaoqiang, CAI Xin, LI Dianzhong, DANG En |
| 图1 淬火态以及不同温度回火后F22M钢的微观组织形貌和位错密度随回火温度的变化 |
| Fig.1 OM (a-e) and TEM (f, g) images of F22M steel after different heat treatments and variation of dislocation density with tempering temperature (h) (dAverage—average width of lath) (a) quenching at 930 oC (b-g) tempering at 610 oC (b), 630 oC (c, f), 650 oC (d, g), and 670 oC (e) |
|