深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺
刘庚, 单以银, 严伟, 苏锐, 任毅, 史显波

Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation
LIU Geng, SHAN Yiyin, YAN Wei, SU Rui, REN Yi, SHI Xianbo
表1 X65钢和Inconel 625合金的本构方程参数
Table 1 Parameters in constitutive equations of X65 steel and Inconel 625 alloy
Materialα / MPa-1n / MPaQ / (J·mol-1)A / S-1
X650.003308.208401.234 × 1035.6039 × 1018
Inconel 6250.002298.563627.884 × 1031.9405 × 1024