深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺 |
| 刘庚, 单以银, 严伟, 苏锐, 任毅, 史显波 |
|
Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation |
| LIU Geng, SHAN Yiyin, YAN Wei, SU Rui, REN Yi, SHI Xianbo |
| 图13 国内某钢厂在终轧温度为850 ℃时热轧后双金属复合板的宏观形貌 |
| Fig.13 Macrostructures of hot-rolled bimetal composite plate by a domestic steel plant at final rolling temperature of 850 oC (a) top view (b) front view |
|