深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺 |
| 刘庚, 单以银, 严伟, 苏锐, 任毅, 史显波 |
|
Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation |
| LIU Geng, SHAN Yiyin, YAN Wei, SU Rui, REN Yi, SHI Xianbo |
| 图10 不同热变形条件下X65钢和Inconel 625合金的反极图(IPF)和大角度晶界(HAGB)图 |
| Fig.10 Inverse pole figures (IPFs) and high-angle grain boundary (HAGB) maps of X65 steel (a-c) and Inconel 625 alloy (d-f) under different thermal deformation conditions (DRX—dynamic recrystallization) (a, d) T = 950 oC, |
|