深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺
刘庚, 单以银, 严伟, 苏锐, 任毅, 史显波

Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation
LIU Geng, SHAN Yiyin, YAN Wei, SU Rui, REN Yi, SHI Xianbo
图7 峰值应力实验值与预测值的拟合结果
Fig.7 Fitting results of experimental and predicted peak stresses (Rc—linear correlation coefficient, eAARE—average relative error)
(a) X65 steel (b) Inconel 625 alloy