深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺
刘庚, 单以银, 严伟, 苏锐, 任毅, 史显波

Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation
LIU Geng, SHAN Yiyin, YAN Wei, SU Rui, REN Yi, SHI Xianbo
图5 不同变形条件下X65钢和Inconel 625合金的峰值应力
Fig.5 Peak stresses of X65 steel and Inconel 625 alloy under different deformation conditions
(a) T = 850 oC (b) T = 950 oC (c) T = 1050 oC (d) T = 1150 oC